Product Name: Jinyang Acrylic Top  
Trade Mark: Jinyang Brand  
Alternative Name: ?  
Molecular formula/Structural Formula:
Production Process: The product is manufactured from acrylic tow by the tow-to-top converter by stretch-breaking method .  
Properties: Good warmth retention property, soft hand, bulky, bright,mildew-proof, anti-moth and good light fastness and thermoelasticity.  
Grade: 3.33,6.67dtex bulky top; 3.33,6.67dtex regular top  
National Standard Grade: ?  
Enterprise Standard Grade: ?  
Specifications:

FJ/T533-85 standard issued by the Ministry of Textile

Items

Unit

1st-grade

2nd-grade

3rd-grade

Test method

sliver weight unevenness

% <=

3.5

5.0

7.0

 
nep(+loose nep) 3.33 dtex

piece/g <=

1.0

2.0

3.0

 
  6.66 dtex

<=

0.8

2.0

3.0

 
flake

piece/m <=

0.5

1.2

1.8

 
percentage of short fibers (<=30mm)

% <=

4.0

5.0

6.0

FJ/T533-85

shrinkage deviation

% +-

2

3

4

 
percentage of long fiber 3.33 dtex>=200mm

% <=

0.5

0.8

1.5

 
  6.66 dtex >=210mm

<=

0.8

1.5

2.0

 
average sliver weigt eviation

g/m +-

1.0

1.5

2.5

 
average length deviation

% +-

7

10

13

 

Remarks:

The performance indexes of regular top are same as bulky top except shrinkage (<=4%)

 
Scope of Application: ?  
Major Applications: 燭o be processed into bulky wool, knitting wool, and ecoration fabrics by unmixed spinning or blend spinning with woo or other chemical fibres. 
Process Method: ?  
Packing: 24 balls wrapped with plastic bags in PP woven bags and tightened with polypropylene strips.  
Packing Size: Net wight: 400kg (central value)
Dimension:10mm?0mm?60mm  
Storage: Separately stored in dry, ventilated warehouse equipped with firefighting facilities according to different lot no., types and grades.  
Transportation: Products in bags are suitable for rail, road and sea transportation.  
Safety Precautions: 1. Keep away from fire and heat sources.
2. Can not be transported or stored together with chemicals of oils, acids and alkai etc.
3. Proper measures should be taken to avoid damages to baling strips during hoisting  